A2 air hardening tool steel annealing heat uniformly to 1650 f.
A2 tool steel heat treat process.
It s highly wear resistant and moderately tough.
The wear resistance properties and cost place a2 between that of o1 and d2 tool steel making it a good all purpose grade for many applications.
Soak at temperature for approximately two hours and cool slowly in the fur nace.
Aisi a2 tool steel is high carbon high alloy tool steel designed to have excellent wear resistance and toughness.
The steel is composted of 1 percent carbon 3 percent silicon 6 percent manganese 5 3 percent chromium 1 1 percent molybdenum and 2 percent vanadium.
A2 tool steel is a 5 chromium medium alloy cold work tool steel possessing sufficient hardenability to be air hardened to 60 rc surface hardness level with good depth of hardening.
A simplified guide to heat treating tool steels when we consider that the greater overall costs of most tools and dies are incurred prior to heat treatment and further that proper heat treatment is critical to the successful application of tooling this so called hardening process is placed in it s proper perspective of importance.
This varies somewhat based on a number of theoretical and practical factors.
A2 tool steel is an air hardening cold work chromium alloy die steel that is preferable to o1 tool steel in applications requiring greater size stability machinability and safer hardening.
A2 tool steel properties.
This widely used tool steel has low distortion in heat treatment good machinability good toughness for severe service high abrasion resistance and deep.
Stress relieving when heavy machining cuts are employed the resultant stresses may be relieved by heating the material to 1200 f to 1250 f for one hour and cooling in still air.
Like d2 it is incredibly resistant to distortion during heat treating and is moderately machinable and grindable.
The prefix a in the name designates it as an air hardening steel.
A2 tool steel is a versatile air hardening tool steel that is characterized by good toughness and excellent dimensional stability in heat treatment a2 is intermediate in wear resistance between o1 oil hardening tool steel and d2 high carbon high chromium tool steel.
A2 steel is an air hardening cold work tool steel.
It is heat treatable and will offer a hardness in the range 57 62 hrc.
Most tool steels grow between about 0 0005 and 0 002 inch per inch of original length during heat treatment.
Generally supplied annealed to hb 231 max.